No.0 PP Sheet Bending Machine

A square PP duct needs four welded seams. This machine folds all four edges from one sheet and leaves a single longitudinal seam — the duct no longer leaks air, the tank no longer leaks water.
What it solves
01Every seam is a leak path and an hour of welding.
Weld, grind, leak-test: the sequence multiplies the cost of a simple duct.
PP corners stress-whiten and crack after a few flex cycles.
Core value
02Four folds, one seam.
Corners that do not whiten.
Ducts from 300 mm side upwards.
How it works
03- 01Buffered bending
The stroke is damped, so stress at the corner stays low and the material does not whiten.
- 02Line heating
Only the fold line softens; surface finish and flatness are untouched.
- 03Four edges in sequence
Ducts and tanks are folded edge by edge with one clamping, leaving one seam.
- 04Duct capability
PP air ducts with a minimum side of 300 mm can be formed directly.
Specifications
04| Sheet thickness | up to 25 mm (0.98 in) |
|---|---|
| Bending length | 1500–3000 mm (4.9 ft–9.8 ft) |
| Bending angle | 60°–180°, adjustable |
| Minimum flange | 50 mm (2.0 in) |
| Power | 6–10 kW |
| Voltage / air | 380 V / 0.5 MPa |
Advantages
05Forming
- Four edges folded from one sheet, one longitudinal seam.
- Corners stay white-free and survive repeated flexing.
- Tanks can be water-tested straight off the machine.
Operation
- Temperature and dwell set by sheet thickness; changing material is a parameter change.
- Automatic and manual modes, foot pedal supported.
- Front and rear stops for repeatable bend lines.
Structure
- Aluminium table and one-piece frame keep long panels straight.
What it bends
06Machine detail


Video
Post a 200 × 200 mm offcut with material and thickness noted; we bend it to your angle and send photos plus video within 48 hours.
Request a trial bendAlso known as
07All names above refer to this machine — see the full alias index.
FAQ
08Can PP ducting be formed directly?
Yes. Four edges are folded from one sheet, leaving one longitudinal seam; ducts from 300 mm side upwards.
Will the corners whiten?
No. The bending stroke is buffered, keeping stress at the corner low.